POLYMER CLASS | Polyesters |
COMMON NAMES | Poly(1,3-propylene succinate), Poly(trimethylene succinate) |
STRUCTURE BASED NAME | Poly(oxypropane-1,3-diyloxybutanedioyl), Poly(oxypropane-1,3-diyloxysuccinyl) |
ACRONYMS | |
CAS # | 28158-21-6 |
CurlySMILES | O{-}CCCOC(=O)CCC{n+}(=O) |
CAS # | 203-740-4, 504-63-2 |
COMMON NAMES | Succinic acid, 1,3-Propanediol |
SMILES | OC(=O)CCC(=O)O.OCCCO |
Std. InChI | InChI=1S/C4H6O4/c5-3(6)1-2-4(7)8/h1-2H2,(H,5,6)(H,7,8).InChI=1S/C3H8O2/c4-2-1-3-5/h4-5H,1-3H2 |
Std. InChIKey | KDYFGRWQOYBRFD-UHFFFAOYSA-N.YPFDHNVEDLHUCE-UHFFFAOYSA-N |
STRUCTURE |
![]() |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molar Volume Vm | mL mol-1 | ||
Density ρ | g mL-1 | ||
Solubility Parameter δ | MPa1/2 | ||
Molar Cohesive Energy Ecoh | J mol-1 | ||
Glass Transition Temperature Tg | K | 232 | |
Molar Heat Capacity Cp | J (mol K)-1 | 288 | |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none |
PROPERTY | UNIT | VALUE / RANGE | PREFERRED |
Molecular Weight of Repeat unit | g mol-1 | 158.15 | |
Van-der-Waals Volume VvW | mL mol-1 | 81.6 | |
Molar Volume Vm | mL mol-1 | 119 - 125 | 122 |
Density ρ | g mL-1 | 1.26 - 1.34 | 1.30 |
Solubility Parameter δ | MPa1/2 | 20.0 - 21.4 | 20.8 |
Molar Cohesive Energy Ecoh | J mol-1 | 48000 - 57400 | 52900 |
Glass Transition Temperature Tg | K | 241- 249 | 245 |
Molar Heat Capacity Cp | J (mol K)-1 | 285 - 292 | 286 (l) |
Entanglement Molecular Weight Me | g mol-1 | ||
Index of Refraction n | none | 1.48 - 1.50 | 1.49 |
Last updated: May 10, 2016